Synced from Product Parameters V2: Basic & Appearance
| Recommended printing conditions | Nozzle Temperature250-270 °CRecommended Nozzle Diameter≥0.2 mmRecommended build surface treatmentPEI or Coating with PVP glueBuild plate temperature100-120 °CChamber Temp80-100°CCooling fan speedoffPrint speed30-120 mm/sRetraction distance1-3 mmRetraction speed1800-3600 mm/minDrying setting100-110℃ for 4-5hAnnealing90℃-4h |
|---|
| | Nozzle Temperature250-270 °CRecommended Nozzle Diameter≥0.2 mmRecommended build surface treatmentPEI or Coating with PVP glueBuild plate temperature100-120 °CChamber Temp80-100°CCooling fan speedoffPrint speed30-120 mm/sRetraction distance1-3 mmRetraction speed1800-3600 mm/minDrying setting100-110℃ for 4-5hAnnealing90℃-4h |
|---|
Printing Tips:1.PC filament is sensitive to moisture and can easily have stringing during printing. To reduce the stringing and surface roughness effectively, keep your filament in a dry box and control relative humidity to below 15%. If the filament has absorbed moisture already, dry the filament in an oven at 100-110°C for 4 hours.2.It is recommended to anneal models printed with PC at 90℃ for 4h, which can effectively release the internal stress and prolong the service life.
No matching print profile files.
Synced from the linked Product Parameters V2 record — use as a starting point for slicing and test prints.
Core temperature, speed and cooling settings from Product Parameters V2.
Nozzle, build plate and pre-print preparation recommendations.
Support material, spacing and compatible material recommendations.
No FAQs for this product yet.
General safety (FusRock)
| How to route filament |
|
||
|---|---|---|---|
| Moisture control |
|
| Short breaks | Store in a sealed dry box or apply a simple vacuum pack; avoid direct sunlight. |
|---|---|
| Long-term storage | Return filament to the factory foil bag, squeeze out air (add a fresh desiccant pack if available), then place inside a household vacuum bag and pull vacuum. Keep in a cool, dry place away from sunlight. |
PTC compact dryer box: 60–70 °C for 4–6 hours.
Small lab oven (forced-air): temperature uniformity is often limited; spools can warp. Reduce temperature/time (example: 40–45 °C for ~4 hours) and cross-check the material-specific drying notes in the datasheet.
Important: if print quality does not improve, test with an empty spool before raising temperature—non-uniform heat can deform plastic flanges.
Large forced-air oven: 60–70 °C for 4–6 hours.
PS: Why do devices differ? Add an internal article or external link (“learn more”).
⚠ Read before drying
(Insert “warped vs normal” spool photos here.)
What moisture does to prints
| Dry | Damp |
|---|---|
| Cleaner surface, stable color, mechanical properties on spec | Pitting, stringing, whitening, weaker properties (material dependent) |
(Optional: 1 / 2 / 3 day exposure at ~80% RH — same test part.)
* Example photos may reference a specific grade (e.g. PAHT-CF); label yours accordingly.
No application disclaimer to display yet. Link a Product Parameters V2 record to this product in the admin.